Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 530 MPa @Temperature 400 °C |
76900 psi @Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 253MA® High Temperature Austenitic Stainless Steel Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be.. |
|||
Tensile Strength, Ultimate | 530 MPa @Temperature 100 °C |
76900 psi @Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu 4318 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled strip/sheet (CPP) and cold rolled strip sheet forms. |
|||
Tensile Strength, Ultimate | 530 MPa @Temperature 427 °C |
76900 psi @Temperature 801 °F |
|
Haynes Multimet® alloy, sand cast, 1171°C heat treatment for 2 hours Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Tensile Strength, Ultimate | 530 MPa | 76900 psi | |
Kennametal Stellite Deloro® 50 Nickel Alloy Nickel base. Provides maximum amount of abrasion and metal-on-metal wear resistance for cast components. Superior wear resistance. Adequate corrosion resistance. Tungsten carbide tools allow for mac.. |
|||
Tensile Strength, Ultimate | 530 MPa | 76900 psi | |
SSAB Tunnplat Domex® 024 BOR Rolled Boron Steel Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron .. |
|||
Tensile Strength, Ultimate | >= 530 MPa | >= 76900 psi | Minimum Guaranteed |
Industeel URANUS® S1 4 % Si, Austenitic Stainless Steel Resistant to Nitric Acid Solutions Description: Research carried out in about the last fifteen years in CREUSOT LOIRE INDUSTRIE laboratories shows that a strong addition of silicon to austenitic stainless steels of the 18/10 type has.. |
|||
Tensile Strength, Ultimate | 530 MPa | 76900 psi | Typical after Solution Annealing |
Industeel UREA 316L Modified 316L Mod Low Si, High Mo Stainless Steel for Urea Plants Description: UREA 316L Modified grade has been specially developed for Urea plant applications. It is a 316L modified stainless steel with extra-low silicon content and substantial higher molybdenum.. |