Polymer Property : Tensile Strength, Ultimate = 530 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 530 MPa

@Temperature 400 °C
76900 psi

@Temperature 752 °F
EN min.; EN 10002-5
Outokumpu 253MA® High Temperature Austenitic Stainless Steel
Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be..
Tensile Strength, Ultimate 530 MPa

@Temperature 100 °C
76900 psi

@Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 4318 Cr-Ni Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled strip/sheet (CPP) and cold rolled strip sheet forms.
Tensile Strength, Ultimate 530 MPa

@Temperature 427 °C
76900 psi

@Temperature 801 °F
Haynes Multimet® alloy, sand cast, 1171°C heat treatment for 2 hours
Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit..
Tensile Strength, Ultimate 530 MPa
76900 psi
Kennametal Stellite Deloro® 50 Nickel Alloy
Nickel base. Provides maximum amount of abrasion and metal-on-metal wear resistance for cast components. Superior wear resistance. Adequate corrosion resistance. Tungsten carbide tools allow for mac..
Tensile Strength, Ultimate 530 MPa
76900 psi
SSAB Tunnplat Domex® 024 BOR Rolled Boron Steel
Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron ..
Tensile Strength, Ultimate >= 530 MPa
>= 76900 psi
Minimum Guaranteed
Industeel URANUS® S1 4 % Si, Austenitic Stainless Steel Resistant to Nitric Acid Solutions
Description: Research carried out in about the last fifteen years in CREUSOT LOIRE INDUSTRIE laboratories shows that a strong addition of silicon to austenitic stainless steels of the 18/10 type has..
Tensile Strength, Ultimate 530 MPa
76900 psi
Typical after Solution Annealing
Industeel UREA 316L Modified 316L Mod Low Si, High Mo Stainless Steel for Urea Plants
Description: UREA 316L Modified grade has been specially developed for Urea plant applications. It is a 316L modified stainless steel with extra-low silicon content and substantial higher molybdenum..