Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 760 MPa
>= 110000 psi
MetalTek C86300 High Tensile Manganese Bronze
High strength and hardness copper-zinc alloy.Applications: Steel mill nuts, ordnance parts, worm gears.Information provided by MetalTekCast UNS C86300; Cast Grade C86300; Cast ASTM B271, B584, B148;..
Tensile Strength, Ultimate >= 760 MPa
>= 110000 psi
MetalTek MTEK 230-B Cast UNS C95500HT Aluminum Bronze
Versatile alloy with high strength, good ductility, unusual toughness, plus exceptional wear resistance. Aluminum Bronze heat treated to higher mechanical properties where necessary.Information prov..
Tensile Strength, Ultimate >= 760 MPa
>= 110000 psi
MetalTek MTEK CA6NM Cast UNS J91540 Martensitic Stainless Steel
"400" series, General corrosion resistant alloys, high strength.Applications: Chemical and food process equipment, jet engine compressor cases and rocket engine parts.Information provided by MetalTe..
Tensile Strength, Ultimate 760 MPa
110000 psi
Haynes Hastelloy® S alloy, weld metal, aged 16000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Tensile Strength, Ultimate 760 MPa
110000 psi
Haynes Hastelloy® S alloy, weld metal, aged 4000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Tensile Strength, Ultimate 760 MPa
110000 psi
Haynes Hastelloy® W alloy, shielded metal arc welds, as-welded
Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica..
Tensile Strength, Ultimate 760 MPa
110000 psi
Haynes HR-120® alloy, solution heat-treated aged at 1200°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Tensile Strength, Ultimate >= 760 MPa
>= 110000 psi
MetalTek IN® 713 UNS N07713 Centri-Vac Nickel Cobalt Based Alloy
Information provided by MetalTek
Tensile Strength, Ultimate 760 MPa

@Temperature 760 °C
110000 psi

@Temperature 1400 °F
Haynes 242® alloy, cold rolled sheet, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Tensile Strength, Ultimate 760 MPa

@Temperature 650 °C
110000 psi

@Temperature 1200 °F
Haynes 625 alloy, cold rolled and 1050°C mill-annealed sheet
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Tensile Strength, Ultimate 760 MPa

@Temperature 205 °C
110000 psi

@Temperature 401 °F
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Tensile Strength, Ultimate 760 MPa
110000 psi
Annealed prior to test
Special Metals BRIGHTRAY® Alloy C Electrical Resistance Alloy
A nickel-chromium electrical-resistance alloy for use at operating temperatures up to 2100°F (1150°C). It contains rare-earth additions for increased oxidation resistance, especially under co..
Tensile Strength, Ultimate 760 MPa

@Temperature 650 °C
110000 psi

@Temperature 1200 °F
Annealed prior to test
Special Metals INCONEL® Alloy 625
Niobium content includes tantalum. A nickel-chromium-molybdenum alloy with an addition of niobium that acts with the molybdenum to stiffen the alloy's matrix and thereby provide high strength witho..
Tensile Strength, Ultimate 760 MPa
110000 psi
Typical
TIMET TIMETAL® 230 Titanium Alloy (Ti-2.5Cu); STA
Cold Formable Medium-Strength AlloyFeatures: This binary, age hardening alloy combines the easy formability and weldability of commercially pure titanium with improved mechanical properties, particu..
Tensile Strength, Ultimate 760 MPa
110000 psi
Typical; Annealed Plate
ATI Allegheny Ludlum AL 2205™ Duplex Stainless Steel, Plate > 0.1875" Duplex Stainless Steel, UNS S31803
Ferromagnetic. The AL 2205 alloy is a nitrogen-enhanced duplex stainless steel alloy. The nitrogen serves to significantly improved the corrosion resistance of the alloy; especially in the welded c..
Tensile Strength, Ultimate 760 MPa
110000 psi
Typical
ATI Allegheny Ludlum AL 400™ Nickel-Base Alloy, Heavily Cold Rolled Sheet and Strip, UNS N04400
Moderately to faintly magnetic at room temperature. Allegheny Ludlum AL 400 alloy is a ductile nickel-copper alloy with resistance to a variety of corrosive conditions. The alloy is most frequentl..
Tensile Strength, Ultimate 760 MPa
110000 psi
ATI Allegheny Ludlum Grade 18 Titanium (UNS R56322)
Uses: heat exchangers, industrial components, tubing.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum.
Tensile Strength, Ultimate 760 MPa
110000 psi
ATI Allegheny Ludlum Grade 9 Titanium (UNS R56320)
Uses: heat exchangers, industrial components, tubing.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum.
Tensile Strength, Ultimate 760 MPa
110000 psi
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367)
The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co..
Tensile Strength, Ultimate 760 MPa
110000 psi
ATI Allvac® AL 6XN® UNS N08367 Specialty Steel
Uses: Process equipment, flue-gas scrubber systems, multi-effect evaporators for brines, seawater, pulp & paper liquors.Property values are for samples in the metallurgical condition: 2050°F anneal..
Tensile Strength, Ultimate >= 760 MPa
>= 110000 psi
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; A (A) Temper; All Sizes (UNS N03360)
Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.
Tensile Strength, Ultimate 760 MPa
110000 psi
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 50% cold work (ASTM XM-8; UNS S43035)
Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi..