Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 74.980 MPa | 10875 psi | ASTM D638 |
Nylene® Mach 6 , Fast Cycle Nylon 6 Description: Nylene® Mach is a fast cycle, high speed, high flow nylon 6. Information provided by Custom Resins.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resourc.. |