Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 74.980 MPa
10875 psi
ASTM D638
Nylene® Mach 6 , Fast Cycle Nylon 6
Description: Nylene® Mach is a fast cycle, high speed, high flow nylon 6. Information provided by Custom Resins.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resourc..