Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nylene® Mach 6 , Fast Cycle Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Nylene®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® Mach 6 , Fast Cycle Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Nylene® Mach is a fast cycle, high speed, high flow nylon 6. Information provided by Custom Resins.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Viscosity Measurement 45
45
relative viscosity, FAV
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 74.980 MPa
10875 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Flexural Modulus 2.899 GPa
420.5 ksi
ASTM D790
Izod Impact, Notched 0.400 J/cm
0.750 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 216 °C
420 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 180 °C
356 °F
ASTM D648