Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 73.8 MPa | 10700 psi | ASTM D638 |
Nylene® Norpex® AX10GF , 10% Glass Reinforced Polyphenylene Ether Description: Norpex® AX10GF is a 10% glass fiber reinforced Polyphenylene Ether. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric.. |
|||
Tensile Strength, Ultimate | 73.8 MPa | 10700 psi | ASTM D638 |
Nylene® Norpex® AX20MR , 20% Mineral Reinforced Polyphenylene Ether Description: Norpex® AX20MR is a 20% mineral reinforced Polyphenylene Ether. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Res.. |