Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 4.83 MPa | 700 psi | |
Valley Adhesives EM-115 High Performance Application Glue Stick Valley Adhesives EM-115 High Performance Application Glue StickHigh peel, shear strength, and heat resistance; Good wetting and heat resistance for potting; Excellent adhesion to wood, plastics, pol.. |
|||
Tensile Strength, Ultimate | 4.83 MPa | 700 psi | |
Dow Corning HV 1760/80 SILICONE RUBBER NATURAL 80 Shore hardness high consistency silicone rubber with fast cure system and excellent tracking and erosion resistanceInformation provided by Dow Corning |
|||
Tensile Strength, Ultimate | 4.83 MPa | 700 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 121-85M100 Thermoplastic Elastomer A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult .. |
|||
Tensile Strength, Ultimate | 4.83 MPa | 700 psi | ASTM D412 |
AdvanSource Biomaterials ChronoPrene™ 40A Thermoplastic Rubber Elastomer ChronoPrene™ is a family of biocompatible thermoplastic elastomeric materialsChronoPrene™ is a family of easy molding, high flow rubber, with excellent chemical resistance to alcohols, acids, and .. |
|||
Tensile Strength, Ultimate | 4.83 MPa | 700 psi | |
Dow Corning 3112 BASE & 1 CATALYST General purpose silicone mold making rubber suited for the reproduction of objects with no deep undercuts or complex shapes. 3112 Base with 1 Catalyst is recommended for use with rigid polyurethane .. |
|||
Tensile Strength, Ultimate | 4.83 MPa @Temperature 121 °C |
700 psi @Temperature 250 °F |
|
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber) Nitrile Rubbers are copolymers of butadiene and acrylonitrile. The term has also been applied to copolymers of other dienes and/or nitriles. Acrylonitrile content may range from 18-50%. Increasin.. |
|||
Tensile Strength, Ultimate | 4.83 MPa | 700 psi | |
Dow Corning 3112 RTV SILICONE RUBBER Moldmaking RTV Rubber; Potting and encapsulating of electrical/electronic productsInformation provided by Dow Corning |
|||
Tensile Strength, Ultimate | 4.83 MPa | 700 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® RT-3840M Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceDisclaimer.. |