Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 2.60 - 65.5 MPa | 377 - 9500 psi | Average value: 34.8 MPa Grade Count:158 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Tensile Strength, Ultimate | 25.5 - 65.5 MPa | 3700 - 9500 psi | Average value: 43.7 MPa Grade Count:9 |
Overview of materials for Styrene/Methyl Methacrylate Copolymer (SMMA) This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Methyl Methacrylate Copolymer (SMMA)". Each property range of values reported is minimum and max.. |