Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 2.60 - 65.5 MPa | 377 - 9500 psi | Average value: 34.8 MPa Grade Count:158 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Tensile Strength, Ultimate | 2.60 MPa | 377 psi | |
Momentive Performance Materials RTV5222 White Adhesive Sealant, Low Modulus Paste One-part totally non-corrosive alkoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: Economical true neu.. |
|||
Tensile Strength, Ultimate | 2.60 MPa | 377 psi | |
Momentive Performance Materials RTV5223 Black Adhesive Sealant, Low Modulus Paste One-part totally non-corrosive alkoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: Economical true neu.. |
|||
Tensile Strength, Ultimate | >= 2.60 MPa | >= 377 psi | ASTM D412 |
Multibase Multi-Flex® TPE A 6221 HR BLK The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 2.60 MPa | 377 psi | |
Momentive Performance Materials RTV5229 Gray Adhesive Sealant, Low Modulus Paste One-part totally non-corrosive alkoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: Economical true neu.. |
|||
Tensile Strength, Ultimate | 2.60 MPa | 377 psi | 508 mm/min; ASTM D638 |
Dow Engage® ENR 7467.00 Ethylene-Butene Copolymer Description: ENR 7467.00 is a high performance ethylene-butene copolymer, offering superior impact properties for more demanding TPO applications. The polymer has very low crystallinity and is avail.. |