Polymer Property : Tensile Strength, Ultimate = 638000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 4400 MPa
638000 psi
Cytec Thornel® T-605/50X 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.12000 filaments/strand.Thornel® products were sold by Amoco and are now owned by Cytec.