Cytec Thornel® T-605/50X 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor

Category Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers
Manufacturer Cytec
Trade Name Thornel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cytec Thornel® T-605/50X 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Amoco Performance Products, Inc.12000 filaments/strand.Thornel® products were sold by Amoco and are now owned by Cytec.
Physical Properties Metric English Comments
Density 1.78 g/cc
0.0643 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 4400 MPa
638000 psi
Modulus of Elasticity 360 GPa
52200 ksi
In Tension
Thermal Properties Metric English Comments
Thermal Conductivity 60.0 W/m-K
416 BTU-in/hr-ft²-°F