Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 4400 MPa | 638000 psi | |
Cytec Thornel® T-605/50X 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.12000 filaments/strand.Thornel® products were sold by Amoco and are now owned by Cytec. |