Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 60900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 420 MPa

@Temperature 200 °C
60900 psi

@Temperature 392 °F
EN min.; EN 10002-5
Outokumpu 4432 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Ultimate 420 MPa

@Temperature 100 °C
60900 psi

@Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 4435 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Tensile Strength, Ultimate 420 MPa

@Temperature 870 °C
60900 psi

@Temperature 1600 °F
Haynes 718 alloy, cold rolled, solution-treated and aged sheet
Cb and Ta content combined weight percentage of 5. Excellent high-temperature strength up to 650°C, good ductility, formability, and weldability. Very good welding characteristics. Applications i..
Tensile Strength, Ultimate 420 - 490 MPa
60900 - 71100 psi
SSAB Tunnplat Aluzink 350A YP High-strength Metal-coated Steel
High-strength Metal-coated SteelComments: Aluzink YP - HSLA steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.4 - 2.0 mm. Iron content is approximate - exact composition is ..
Tensile Strength, Ultimate <= 420 MPa
<= 60900 psi
SSAB Tunnplat Aluzink B420A Metal-coated Mild Steel
Metal-coated Mild SteelComments: Aluzink - Aluminum-zinc coated sheet. Property values are for thicknesses 0.4 - 2.00 mm. Iron content is approximate - exact composition is not reported by the manu..
Tensile Strength, Ultimate <= 420 MPa
<= 60900 psi
SSAB Tunnplat Aluzink F26A Metal-coated Mild Steel
Metal-coated Mild SteelComments: Aluzink - Aluminum-zinc coated sheet. Property values are for thicknesses 0.4 - 2.00 mm. Iron content is approximate - exact composition is not reported by the manu..
Tensile Strength, Ultimate 420 - 500 MPa
60900 - 72500 psi
SSAB Tunnplat Docol® 300 BH High-strength Steel
High-strength SteelComments: Docol BH - Cold Rolled Steel - rephosphorized steel with bake hardening effect. Property values are for cold-rolled steel; thicknesses 0.40 - 2.0 mm. Iron content is ap..
Tensile Strength, Ultimate 420 - 500 MPa
60900 - 72500 psi
SSAB Tunnplat Docol® 300 RP High-strength Steel
High-strength SteelComments: Docol RP - Cold Rolled Steel - rephosphorized steel. Property values are for cold-rolled steel; thicknesses 0.40 - 3.0 mm. Iron content is approximate - exact compositi..
Tensile Strength, Ultimate 420 - 490 MPa
60900 - 71100 psi
SSAB Tunnplat Dogal 350YP High-strength Metal-coated Steel
High-strength Metal-coated SteelComments: Dogal YP - HSLA steel. Property values are for thicknesses 0.4 to 2.5 mm. Iron content is approximate - exact composition is not reported by the manufactur..
Tensile Strength, Ultimate <= 420 MPa
<= 60900 psi
SSAB Tunnplat Dogal B420 Metal-coated Mild Steel
Metal-coated Mild SteelComments: Dogal - Hotdipped-galvanized sheet. Property values are for thicknesses 0.5 - 2.5 mm. Iron content is approximate - exact composition is not reported by the manufac..
Tensile Strength, Ultimate <= 420 MPa
<= 60900 psi
SSAB Tunnplat Dogal F26 Metal-coated Mild Steel
Metal-coated Mild SteelComments: Dogal - Hotdipped-galvanized sheet. Property values are for thicknesses 0.5 - 2.5 mm. Iron content is approximate - exact composition is not reported by the manufac..
Tensile Strength, Ultimate >= 420 MPa
>= 60900 psi
SSAB Tunnplat Domex® 350XP Extra High-strength Cold-forming Steel
Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene..
Tensile Strength, Ultimate >= 420 MPa
>= 60900 psi
SSAB Tunnplat Domex® 350YP Cold-forming Steel, HSLA
Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. General use of Domex®..
Tensile Strength, Ultimate 420 MPa
60900 psi
Wieland 1023 Wilaform Gold
Hard yellow gold alloy with good extensibility. Particularly suitable for by machine manufactured decoration.Applications: casting, chains, coin/shape, laminar decorationDental
Tensile Strength, Ultimate 420 MPa
60900 psi
Wieland 1101 Wilaform Gold
Hard yellow gold alloy with good extensibility. Universally applicable in decoration manufacturing.Applications: casting, chainsDental
Tensile Strength, Ultimate <= 420 MPa
<= 60900 psi
Wire
CLAL-MSX ARCAP Anticorrosion AP1 0 Annealed, Drawn Copper Alloy
Description: The AP1D grade has been developed especially for being machined by lathe. Its machineability is one of the best of all of the corrosion resistant alloys. The very good machineability of..
Tensile Strength, Ultimate 420 - 500 MPa
60900 - 72500 psi
CLAL-MSX NICLAFOR® 1000 TB Quenched Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Tensile Strength, Ultimate 420 - 480 MPa
60900 - 69600 psi
Wire
CLAL-MSX ARCAP Anticorrosion AP1 H11 1/4 hard, Drawn Copper Alloy
Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin..
Tensile Strength, Ultimate 420 - 480 MPa
60900 - 69600 psi
ArcelorMittal 300 BH Bake hardening steel, Cold rolled
Available in the following: uncoated (HC300B), electroglavanized (HC300B+ZE) and Extragal®/Galvannealed (HC300BD+Z)Description: The composition and processing of these steels are designed to promot..
Tensile Strength, Ultimate 420 - 490 MPa
60900 - 71100 psi
ArcelorMittal HSLA 340 High strength low alloy steel for cold forming, Cold Rolled
Available in the following: uncoated (HC340LA), electroglavanized (HC340LA +ZE) and Extragal®/galfan/Galvannealed (HC340LA+Z/+ZA/+ZF)Description: Steels in the HSLA (High Strength Low Alloy) range ..