Category Metal , Ferrous Metal , Stainless Steel , T 400 Series Stainless Steel
Manufacturer Ametek
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ametek P409L P/M Stainless Steel, Sintered from 6.60 g/cc Green Density.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
P409L is a ferritic, weldable grade of stainless steel with high compressibility, enhanced green strength and good sinterability. This stabilized grade provides excellent corrosion resistance and has the capacity to provide high caliber mechanical properties because of its high temperature sintering response. P409L may be used in automotive exhaust system applications, among other uses.For property data reported here: Compacting properties measured on powders with 1% lithium stearate. Sintering was done in dissociated ammonia at 1121°C (2050°F) for 45 minutes. Compacting pressure 50 tsi. Green strength 2200 psi. Sintered breaking strength 120,000 psi.Information provided by Ametek Specialty Metal Products.
Physical Properties Metric English Comments
Bulk Density 2.80 g/cc
0.101 lb/in³
Powder
Density 6.67 g/cc
0.241 lb/in³
Sintered
Mechanical Properties Metric English Comments
Hardness, Rockwell B 80
80
Tensile Strength, Ultimate 441 MPa
64000 psi
Elongation at Break 5.3 %
5.3 %
Thermal Properties Metric English Comments
Shrinkage 0.24 %
0.24 %
versus die size
Component Elements Properties Metric English Comments
Carbon, C <= 0.030 %
<= 0.030 %
Chromium, Cr 11.5 - 13.5 %
11.5 - 13.5 %
Iron, Fe 82.4 - 88.5 %
82.4 - 88.5 %
As Remainder
Manganese, Mn <= 2.0 %
<= 2.0 %
Phosphorous, P <= 0.040 %
<= 0.040 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.030 %
<= 0.030 %
Descriptive Properties Value Comments
Powder Flow 30 sec/50 g