Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 340 - 420 MPa | 49300 - 60900 psi | |
SSAB Tunnplat Aluzink 220A RP-X High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Aluzink RP - rephosphorized steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.5 - 1.5 mm. Iron content is approximate - exact compo.. |
|||
Tensile Strength, Ultimate | 350 - 420 MPa | 50800 - 60900 psi | |
SSAB Tunnplat Aluzink 280A YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Aluzink YP - HSLA steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.4 - 2.0 mm. Iron content is approximate - exact composition is .. |
|||
Tensile Strength, Ultimate | 340 - 420 MPa | 49300 - 60900 psi | |
SSAB Tunnplat Docol® 220 BH High-strength Steel High-strength SteelComments: Docol BH - Cold Rolled Steel - rephosphorized steel with bake hardening effect. Property values are for cold-rolled steel; thicknesses 0.40 - 2.0 mm. Iron content is ap.. |
|||
Tensile Strength, Ultimate | 340 - 420 MPa | 49300 - 60900 psi | |
SSAB Tunnplat Docol® 220 RP High-strength Steel High-strength SteelComments: Docol RP - Cold Rolled Steel - rephosphorized steel. Property values are for cold-rolled steel; thicknesses 0.40 - 3.0 mm. Iron content is approximate - exact compositi.. |
|||
Tensile Strength, Ultimate | 340 - 420 MPa | 49300 - 60900 psi | |
SSAB Tunnplat Dogal 180 RP-X High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal RP - rephosphorized. Iron content is approximate - exact composition is not reported by the manufacturer.Data provided by SSAB Tunnplat. |
|||
Tensile Strength, Ultimate | 340 - 420 MPa | 49300 - 60900 psi | |
SSAB Tunnplat Dogal 220 RP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal RP - rephosphorized. Iron content is approximate - exact composition is not reported by the manufacturer.Data provided by SSAB Tunnplat. |
|||
Tensile Strength, Ultimate | 340 - 420 MPa | 49300 - 60900 psi | |
SSAB Tunnplat Dogal 220 RP-X High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal RP - rephosphorized. Iron content is approximate - exact composition is not reported by the manufacturer.Data provided by SSAB Tunnplat. |
|||
Tensile Strength, Ultimate | 350 - 420 MPa | 50800 - 60900 psi | |
SSAB Tunnplat Dogal 260YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal YP - HSLA steel. Property values are for thicknesses 0.4 to 2.5 mm. Iron content is approximate - exact composition is not reported by the manufactur.. |
|||
Tensile Strength, Ultimate | 350 - 420 MPa | 50800 - 60900 psi | |
SSAB Tunnplat Dogal 280YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal YP - HSLA steel. Property values are for thicknesses 0.4 to 2.5 mm. Iron content is approximate - exact composition is not reported by the manufactur.. |
|||
Tensile Strength, Ultimate | 300 - 420 MPa | 43500 - 60900 psi | |
ArcelorMittal 12 High formability steel for drawing, Hot rolled Available in the following: uncoated (DD12) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used extensively in the au.. |
|||
Tensile Strength, Ultimate | 270 - 420 MPa | 39200 - 60900 psi | |
ArcelorMittal 52+AS Aluminized steel Use: Average drawingInformation provided by ArcelorMittal |