ArcelorMittal 52+AS Aluminized steel

Category Metal , Ferrous Metal , Alloy Steel
Manufacturer ArcelorMittal
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ArcelorMittal 52+AS Aluminized steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Use: Average drawingInformation provided by ArcelorMittal
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 270 - 420 MPa
39200 - 60900 psi
Tensile Strength, Yield 140 - 300 MPa
20300 - 43500 psi
Elongation at Break >= 26 %
>= 26 %
80 mm