Polymer Property : Tensile Strength, Ultimate = 40000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 241 - 276 MPa
35000 - 40000 psi
Brass butt joint
Lucas-Milhaupt SIL-FOS 5 Silver/ Copper/ Phosphorus Alloy
Applications: Sil-Fos 5 was developed primarily for use on copper, but their use has extended to other nonferrous copper base alloys. It is used extensively on refrigeration units, air conditionin..
Tensile Strength, Ultimate 241 - 276 MPa
35000 - 40000 psi
Brass butt joint
Lucas-Milhaupt SIL-FOS Silver/ Copper/ Phosphorus Alloy
Applications: Sil-Fos was developed primarily for use on copper, but their use has extended to other nonferrous copper base alloys. It is used extensively on refrigeration units, air conditioning ..
Tensile Strength, Ultimate 241 - 276 MPa
35000 - 40000 psi
Nickel-Silver butt joint
Lucas-Milhaupt SIL-FOS Silver/ Copper/ Phosphorus Alloy
Applications: Sil-Fos was developed primarily for use on copper, but their use has extended to other nonferrous copper base alloys. It is used extensively on refrigeration units, air conditioning ..
Tensile Strength, Ultimate 255 - 276 MPa
37000 - 40000 psi
Eagle Brass 151 ZHC® COPPER, Annealed
Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c..
Tensile Strength, Ultimate 234 - 276 MPa
34000 - 40000 psi
Eagle Brass 210 Gilding Metal, Annealed
CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi..