Tensile Strength, Ultimate 2.69 MPa
390 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 201-68W228 Thermoplastic Elastomer  (discontinued **)
A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated for low density foamed profile extrusion applications and has lon..
Tensile Strength, Ultimate 2.69 MPa
390 psi
Dow Corning HM-2510 CLEAR ASSEMBLY SEALANT
A reactive Hot Melt silicone sealant that has immediate strength and crosslinks into a neutral cure RTV sealantInformation provided by Dow Corning
Tensile Strength, Ultimate 2.69 MPa
390 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 251-70W232 Thermoplastic Elastomer
A soft, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and contains non-ether brominated flame retard..
Tensile Strength, Ultimate 2.69 MPa
390 psi
ASTM D412; ISO 37
Advanced Polymer Alloys DuraGrip™ DGR 6040 NCEHT Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6040NCEHT is a general purpose Thermoplastic Elastomer (TPE) designed to process easily in injection molding and extrusion. It features excellent soft touch feel with improved surface..
Tensile Strength, Ultimate 2.69 MPa
390 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 181-64MED Thermoplastic Elastomer  (discontinued **)
A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grades. ..
Tensile Strength, Ultimate 2.69 MPa
390 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 201-64W175 Thermoplastic Elastomer  (discontinued **)
A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for thin wall ..
Tensile Strength, Ultimate 2.69 MPa
390 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 221-64W175 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed ..