Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Santoprene® 201-68W228 Thermoplastic Elastomer  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 201-68W228 Thermoplastic Elastomer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated for low density foamed profile extrusion applications and has long term sealability, low temperature flexibility and heat weldability. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for extrusion. It is polyolefin based and completely recyclable.Water can be used as physical foaming agent. Recommended for applications requiring excellent ozone resistance.Information provided by Advanced Elastomer Systems
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 68
68
.12 in; ASTM D2240
Tensile Strength at Break 6.89 MPa
1000 psi
Across Flow; ASTM D412
Tensile Strength, Ultimate 2.69 MPa
390 psi
Across Flow; ASTM D412
Elongation at Break 450 %
450 %
Across Flow; ASTM D412
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Drying Temperature 82.2 °C
180 °F
Dry Time 3 hour
3 hour
Descriptive Properties Value Comments
Change in Mass in IRM 903 Oil at 257°F for 70 hr 87
Color Natural Color
Form Pellets