Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 2.69 MPa | 390 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 201-68W228 Thermoplastic Elastomer
(discontinued **) A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated for low density foamed profile extrusion applications and has lon.. |
|||
Tensile Strength, Ultimate | 2.69 MPa | 390 psi | |
Dow Corning HM-2510 CLEAR ASSEMBLY SEALANT A reactive Hot Melt silicone sealant that has immediate strength and crosslinks into a neutral cure RTV sealantInformation provided by Dow Corning |
|||
Tensile Strength, Ultimate | 2.69 MPa | 390 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 251-70W232 Thermoplastic Elastomer A soft, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and contains non-ether brominated flame retard.. |
|||
Tensile Strength, Ultimate | 2.69 MPa | 390 psi | ASTM D412; ISO 37 |
Advanced Polymer Alloys DuraGrip™ DGR 6040 NCEHT Thermoplastic Elastomer (TPE) DuraGrip® DGR 6040NCEHT is a general purpose Thermoplastic Elastomer (TPE) designed to process easily in injection molding and extrusion. It features excellent soft touch feel with
improved surface.. |
|||
Tensile Strength, Ultimate | 2.69 MPa | 390 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 181-64MED Thermoplastic Elastomer
(discontinued **) A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grades. .. |
|||
Tensile Strength, Ultimate | 2.69 MPa | 390 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 201-64W175 Thermoplastic Elastomer
(discontinued **) A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for thin wall .. |
|||
Tensile Strength, Ultimate | 2.69 MPa | 390 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 221-64W175 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed .. |