Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 370 MPa

@Temperature 300 °C
53700 psi

@Temperature 572 °F
EN min.; EN 10002-5
Outokumpu 4435 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Tensile Strength, Ultimate 370 MPa

@Temperature 500 °C
53700 psi

@Temperature 932 °F
EN min.; EN 10002-5
Outokumpu 4828 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
Tensile Strength, Ultimate 370 MPa

@Temperature 500 °C
53700 psi

@Temperature 932 °F
EN min.; EN 10002-5
Outokumpu 4833 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
Tensile Strength, Ultimate 370 MPa

@Temperature 500 °C
53700 psi

@Temperature 932 °F
EN min.; EN 10002-5
Outokumpu 4845 High Temperature Austenitic Stainless Steel
Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o..
Tensile Strength, Ultimate 370 MPa

@Temperature 200 °C
53700 psi

@Temperature 392 °F
EN min.; EN 10002-5
Outokumpu 4878 High Temperature Austenitic Stainless Steel
Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For ..
Tensile Strength, Ultimate 370 MPa

@Temperature 870 °C
53700 psi

@Temperature 1600 °F
Haynes 25 alloy, hot rolled and 1230°C solution annealed sheet
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Ultimate 370 - 450 MPa
53700 - 65300 psi
SSAB Tunnplat Docol® 280YP High-strength Steel
High-strength SteelComments: Docol YP - Cold Rolled Steel - HSLA. Property values are for cold-rolled steel; thicknesses 0.5 - 3.00 mm. Iron content is approximate - exact composition is not report..
Tensile Strength, Ultimate 370 - 470 MPa
53700 - 68200 psi
CLAL-MSX ARCAP Anticorrosion AP1 H11 1/4 hard, Rolled Copper Alloy
Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin..
Tensile Strength, Ultimate >= 370 MPa
>= 53700 psi
Aleris Alustar Aluminum Alloy, H321/H116; 2 - 20 mm thickness
At least 20% stronger than AA 5083 before and after welding. Bendability and weldability similar to AA 5083. High corrosion resistance. Provides options for ship design and building.Composition d..
Tensile Strength, Ultimate 370 MPa
53700 psi
Ametek P303L P/M Stainless Steel, Sintered from 6.7 g/cc Green Density
Powder apparent bulk density 2.8 g/cc; powder flow 30 sec/50g.Compacting properties measured on powders with 1% lithium stearate. Sintering was done in dissociated ammonia at 1121°C (2050°F) for ..
Tensile Strength, Ultimate 370 MPa
53700 psi
Ametek P410L P/M Stainless Steel, Sintered from 6.45 g/cc Green Density
Powder apparent bulk density 2.8 g/cc; powder flow 30 sec/50g.Compacting properties measured on powders with 1% lithium stearite. Sintering was done in dissociated ammonia at 1121°C (2050°F) for ..
Tensile Strength, Ultimate 370 MPa
53700 psi
Ametek Ultra 316L P/M Stainless Steel, Sintered from 6.8 g/cc Green Density
Ametek's patented Ultra Stainless Steels™ are produced by alloying the conventional austenitic compositions with a small amount of a copper-nickel-tin alloy. This results in a marked improvement i..
Tensile Strength, Ultimate 370 - 430 MPa
53700 - 62400 psi
ArcelorMittal 260 BH Bake hardening steel, Cold rolled
Available in the following: uncoated (HC260B), electroglavanized (HC260B+ZE) and Extragal®/Galvannealed (HC260BD+Z)Description: The composition and processing of these steels are designed to promot..
Tensile Strength, Ultimate >= 370 MPa
>= 53700 psi
Minimum
Aleris Weldural Aluminum Alloy, 200 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..
Tensile Strength, Ultimate 370 - 390 MPa
53700 - 56600 psi
Rm
ALIMEX 2017A T451 Aluminum Alloy Rolled
Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHSolution heat treated, stress relieved by stretching a controlled amount and then naturally aged.
Tensile Strength, Ultimate 370 MPa
53700 psi
ASTM E8
M Cubed Technologies ASC-301 Aluminum alloy-30% SiC Metal Matrix Composite
High stiffness, low density composite. Parts are cast using several standard foundry techniques Size range varies from small components (1lb or smaller) to parts greater than 10 ft. square with co..