Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 280 - 450 MPa | 40600 - 65300 psi | |
Materion Brush 1915â„¢ Hard Temper Wire, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Tensile Strength, Ultimate | 300 - 450 MPa | 43500 - 65300 psi | |
MMCC Al/Al2O3 Short Fiber Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Tensile Strength, Ultimate | 280 - 450 MPa | 40600 - 65300 psi | |
Materion Brush 1915â„¢ Hard Temper Rod, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Tensile Strength, Ultimate | 300 - 450 MPa | 43500 - 65300 psi | |
MMCC Al/SiC Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Tensile Strength, Ultimate | 370 - 450 MPa | 53700 - 65300 psi | |
SSAB Tunnplat Docol® 280YP High-strength Steel High-strength SteelComments: Docol YP - Cold Rolled Steel - HSLA. Property values are for cold-rolled steel; thicknesses 0.5 - 3.00 mm. Iron content is approximate - exact composition is not report.. |
|||
Tensile Strength, Ultimate | 400 - 450 MPa | 58000 - 65300 psi | Rod |
CLAL-MSX ARCAP Anticorrosion AP1 H11 1/4 hard, Drawn Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Tensile Strength, Ultimate | 390 - 450 MPa | 56600 - 65300 psi | |
ArcelorMittal HSLA 300 High strength low alloy steel for cold forming, Cold Rolled Available in the following: uncoated (HC300LA), electroglavanized (HC300LA +ZE) and Extragal®/galfan/Galvannealed (HC300LA+Z/+ZA/+ZF)Description: Steels in the HSLA (High Strength Low Alloy) range .. |