Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | ASTM D638 |
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 20 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | ASTM D638 |
Global GA-3245 High Density Polyethylene, Film Extrusion Grade
(discontinued **) Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- shopping bags, packing bagsInformation provided by Global Polymers Corporation. |
|||
Tensile Strength, Ultimate | 37.0 MPa @Temperature 120 °C |
5370 psi @Temperature 248 °F |
ISO 527 |
LATI LASULF Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | ASTM D638 |
Solvay Specialty Polymers Algoflon® S 111 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type IV.G.1 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p.. |
|||
Tensile Strength, Ultimate | 37.0 - 74.0 MPa | 5370 - 10700 psi | Average value: 58.8 MPa Grade Count:4 |
Overview of materials for Ethylene Vinyl Alcohol (EVOH) This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Tensile Strength, Ultimate | 37.0 - 60.0 MPa | 5370 - 8700 psi | Average value: 51.9 MPa Grade Count:21 |
Overview of materials for Phenolic, Novolac, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Flock Filled". Each property range of values reported is minimum and maximum .. |
|||
Tensile Strength, Ultimate | 37.0 MPa @Temperature 22.0 °C |
5370 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® BMC 0800 Unsaturated Polyester UP BMC 0800 is a special SMC for applications within household and kitchenware. The glass level has been selected to combine good mould ability with good strength and stiffness properties. The product .. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | |
Kuraray HYBRAR® PH5 Polypropylene Blend Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | ASTM D638 |
Stratasys® ABSi Stratasys is the only company that gives engineers the ability to manufacture real ABSi industrial thermoplastic parts direct from digital files. ABSi parts can be used from conceptual prototyping t.. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | 2 in/min, at max load; ASTM D638 |
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 37.0 - 50.0 MPa | 5370 - 7250 psi | ASTM D638 |
Zeus ETFE Tubing ETFE (Ethylenetetrafluoroethylene), a copolymer of ethylene and tetrafluoroethylene, is used in applications requiring excellent impact, abrasion and stress cracking resistance. This polymer possess.. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | 2 in/min, at max load; ASTM D638 |
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | DIN 53504 |
Lubrizol ESTANE® 5702F3 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | DIN 53504 |
Lubrizol ESTANE® 58610 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | DIN 53504 |
Lubrizol ESTANE® ETE50DT3 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | DIN 53504 |
Lubrizol ESTANE® 54610 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | ISO 527 |
DSM Fibre Intermediates Nyrim® 3000 (Dry) Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) tec.. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | ASTM D638 |
DuPont™ Surlyn® 8140 Ionomer Resin, Sodium Surlyn® 8140 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | ISO R527 |
Arkema Group ORGASOL® 2002 D Nat 1 Polyamide 12, Food Contact Approved Information provided by Arkema Group |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | ASTM D412 |
BASF Elastollan® C-78A Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen.. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | Z; ASTM D638 |
ALM PA 605-A Filled Nylon 12 Prototyping Polymer 50% Aluminum filled nylon 12 that can produce accurate parts with excellent part strength and surface detail.Drop in replacement for other commercially available 50% aluminum filled materials with a.. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | Z; ASTM D638 |
ALM PA-840-GSL Filled Nylon 12 Prototyping Polymer Engineered for excellent mechanical properties, part definition and surface finish.Stabilized against thermal degradation resulting in little or no scrap material, with typical virgin refresh rates .. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | ASTM D412 |
BASF Elastollan® 1190A Polyether Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes... |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | |
Alliance BCN-10 Bonded (Composite) Magnetic Material |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | |
Alliance BCN-12 Bonded (Composite) Magnetic Material |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | |
Alliance BCN-14 Bonded (Composite) Magnetic Material |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | |
Alliance BCN-17 Bonded (Composite) Magnetic Material |
|||
Tensile Strength, Ultimate | 37.0 MPa @Temperature 900 °C |
5370 psi @Temperature 1650 °F |
|
Resistalloy International Fecralloy™ Electrical Resistance Steel Yttrium addition does not appear in nominal composition. Ferritic stainless steel with aluminum. Available as wire, bar, tube, and strip. Used mainly for electrical elements in both industrial and.. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | ASTM D638 |
Plenco 7591 Phenolic, Pellet, Transfer Molded PLENCO 07591 is a mineral and flock cotton filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |