Stratasys® ABSi

Category Polymer , Rapid Prototyping Polymer , Thermoplastic , ABS Polymer
Manufacturer Stratasys
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Stratasys® ABSi.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Stratasys is the only company that gives engineers the ability to manufacture real ABSi industrial thermoplastic parts direct from digital files. ABSi parts can be used from conceptual prototyping through design verification through direct digital manufacturing. It’s strength is superior to ABS and the translucent nature of ABSi is beneficial for monitoring material flow and light transmission, most commonly used for medical and automotive applications. When combined with Stratasys FDM (Fused Deposition Modeling) systems, ABSi gives you Real Parts™ that are visually unique, dimensionally accurate, durable and hold shape over time.Information provided by Stratasys®
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength, Ultimate 37.0 MPa
5370 psi
ASTM D638
Elongation at Break 3.1 %
3.1 %
ASTM D638
Tensile Modulus 1.915 GPa
277.7 ksi
ASTM D638
Flexural Strength 61.0 MPa
8850 psi
ASTM D790
Flexural Modulus 1.82 GPa
264 ksi
ASTM D790
Izod Impact, Notched 1.014 J/cm
1.900 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.189 J/cm
4.101 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 121 µm/m-°C

@Temperature 20.0 °C
67.2 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °C
189 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 73.0 °C
163 °F
ASTM D648
Glass Transition Temp, Tg 116 °C
241 °F
DSC (SSYS)
Flammability, UL94 HB
HB