Polymer Property : Tensile Strength, Ultimate = 321.64 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 55.0 - 321.64 MPa

@Temperature -40.0 - 150 °C
7980 - 46650 psi

@Temperature -40.0 - 302 °F
Average value: 139 MPa Grade Count:4
Overview of materials for Nylon 6, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E..