Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | Cured |
KKPC Kumho RM 21L High Styrene Resin Masterbatch (HSR) High Styrene Resin Masterbatch (HSR)Characteristics: KOSYN KHS is produced by mixing SBR 1502 of 23.5% styrene and high styrene resin latex at high temperature. It works as plasticizer which improve.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | |
Sylvin Technologies 9604-95 Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | |
Williams Advanced Alloys WS96 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | ASTM D638 |
CPC - Vycom SEABOARD™ LITE High density polyethylene (HDPE) Seaboard Lite is a high density polyethylene (HDPE) sheet formulated to meet the specific requirements of marine and other outdoor environments. Seaboard Lite is UV stable and will withstand the ele.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | ASTM D412 |
Colorite Polymers CS1533UL Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | ASTM D412 |
Colorite Polymers CS9034SR Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | ASTM D638 |
Colorite Polymers 9000 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | ASTM D638 |
Colorite Polymers 9002 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | ASTM D638 |
Colorite Polymers 9077 Non-Phthalate 77 Series Vinyl Compound Description: The Colorite 77 series is a family of compounds designed for those medical device producers that require the use of a non-phthalate plasticizer that has superior resistance to extractio.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | ASTM D638 |
Colorite Polymers 9813 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | ASTM D412 |
Colorite Polymers CS1535UL Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | Bond strength to glass |
Dymax Light Weld® 426 High Clarity Glass Bonding Adhesive Glass Bonding in SecondsDescriptionDymax Light Weld® 400 Series adhesives form high-clarity, invisible bonds between glass and other substrates in seconds. In addition to many structural glass bond.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | ASTM D638 |
Arkema Group Solarkote® P-600 Acrylic PVC Capstock, clear, high glossInformation provided by Arkema Group |