Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 162 MPa | 23500 psi | ISO 527-1, 2 |
Polyplastics Duranex® 3405 Polybutylene Terephthalate (PBT), Standard, 45% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Tensile Strength, Ultimate | 162 MPa | 23500 psi | Annealed |
CMW® D158F Silver Graphite Contact Material For electrical contacts; reduced sticking, low frictionInformation provided by CMW Inc. |
|||
Tensile Strength, Ultimate | 162 MPa | 23500 psi | ATSM D638 |
Ashley Polymers Ashlene® 630-33G Nylon 6, 33% Glass Reinforced Nylon 6, 33% glass reinforced resin.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 162 MPa | 23500 psi | ASTM D638 |
A. Schulman ComAlloy Lubrilon® 632 Nylon 6/6, Carbon Fiber/PTFE Filled Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |