Polymer Property : Tensile Strength, Ultimate = 162 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 162 MPa
23500 psi
ISO 527-1, 2
Polyplastics Duranex® 3405 Polybutylene Terephthalate (PBT), Standard, 45% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Tensile Strength, Ultimate 162 MPa
23500 psi
Annealed
CMW® D158F Silver Graphite Contact Material
For electrical contacts; reduced sticking, low frictionInformation provided by CMW Inc.
Tensile Strength, Ultimate 162 MPa
23500 psi
ATSM D638
Ashley Polymers Ashlene® 630-33G Nylon 6, 33% Glass Reinforced
Nylon 6, 33% glass reinforced resin.Data provided by the manufacturer
Tensile Strength, Ultimate 162 MPa
23500 psi
ASTM D638
A. Schulman ComAlloy Lubrilon® 632 Nylon 6/6, Carbon Fiber/PTFE Filled
Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma..