CMW® D158F Silver Graphite Contact Material

Category Metal , Metal Matrix Composite , Nonferrous Metal , Precious Metal , Silver Alloy
Manufacturer CMW Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMW® D158F Silver Graphite Contact Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For electrical contacts; reduced sticking, low frictionInformation provided by CMW Inc.
Physical Properties Metric English Comments
Density 10.12 g/cc
0.3656 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell F 36 - 69
36 - 69
36 (annealed) - 69 (worked)
Tensile Strength, Ultimate 162 MPa
23500 psi
Annealed
241 MPa
35000 psi
Worked
Thermal Properties Metric English Comments
Melting Point <= 980 °C
<= 1800 °F
Liquidus 980 °C
1800 °F
Component Elements Properties Metric English Comments
Carbon, C 1.0 %
1.0 %
Silver, Ag 99 %
99 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000174 ohm-cm
0.00000174 ohm-cm
(99% IACS)