Polymer Property : Tensile Strength, Ultimate = 20.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 20.0 - 20.0 MPa

@Temperature 60.0 - 60.0 °C
2900 - 2900 psi

@Temperature 140 - 140 °F
Average value: 20.0 MPa Grade Count:1
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor..
Tensile Strength, Ultimate 0.903 - 20.0 MPa
131 - 2900 psi
Average value: 8.71 MPa Grade Count:24
Overview of materials for PVC, Foam Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Foam Grade". Each property range of values reported is minimum and maximum values of appropriate Ma..
Tensile Strength, Ultimate 15.0 - 20.0 MPa
2180 - 2900 psi
Biomer P209 PHB Biodegradable Polymer
PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula of the subunit is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. P..
Tensile Strength, Ultimate 18.0 - 20.0 MPa
2610 - 2900 psi
Biomer P240 PHB Biodegradable Polymer
PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula of the subunit is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. P..