Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 1205 MPa
>= 174800 psi
MetalTek IN® 909 Centri-Vac Nickel Cobalt Based Alloy
Information provided by MetalTek
Tensile Strength, Ultimate 1205 MPa
174800 psi
Typical
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Fastener Stock
Medium To High Strength General-Purpose Alloy. Tensile property data below is typical of fastener stock; more specific form/thickness entries are also available in MatWeb.Industry Specifications: ..
Tensile Strength, Ultimate 1205 MPa
174800 psi
Typical
TIMET 6-6-2 Titanium Alloy (Ti-6Al-6V-2Sn), Solution Treated and Aged
Features: TIMETAL 6-6-2 offers improved strength properties and greater depth hardenability compared with TIMETAL 6-4.Data provided by TIMET.
Tensile Strength, Ultimate 1205 MPa

@Treatment Temp. 760 °C,
Time 1.44e+7 sec
174800 psi

@Treatment Temp. 1400 °F,
Time 4000 hour
Room temp test after thermal exposure
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened, after long term high temperature exposure
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b..