Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | >= 1205 MPa | >= 174800 psi | |
MetalTek IN® 909 Centri-Vac Nickel Cobalt Based Alloy Information provided by MetalTek |
|||
Tensile Strength, Ultimate | 1205 MPa | 174800 psi | Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Fastener Stock Medium To High Strength General-Purpose Alloy. Tensile property data below is typical of fastener stock; more specific form/thickness entries are also available in MatWeb.Industry Specifications: .. |
|||
Tensile Strength, Ultimate | 1205 MPa | 174800 psi | Typical |
TIMET 6-6-2 Titanium Alloy (Ti-6Al-6V-2Sn), Solution Treated and Aged Features: TIMETAL 6-6-2 offers improved strength properties and greater depth hardenability compared with TIMETAL 6-4.Data provided by TIMET. |
|||
Tensile Strength, Ultimate | 1205 MPa @Treatment Temp. 760 °C, Time 1.44e+7 sec |
174800 psi @Treatment Temp. 1400 °F, Time 4000 hour |
Room temp test after thermal exposure |
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened, after long term high temperature exposure Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b.. |