MetalTek IN® 909 Centri-Vac Nickel Cobalt Based Alloy

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer MetalTek
Trade Name IN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek IN® 909 Centri-Vac Nickel Cobalt Based Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MetalTek
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 1205 MPa
>= 174800 psi
Tensile Strength, Yield >= 965 MPa
>= 140000 psi
Elongation at Break >= 8.0 %
>= 8.0 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.060 %
<= 0.060 %
Cobalt, Co 12 - 16 %
12 - 16 %
Iron, Fe 36.44 - 47.4 %
36.44 - 47.4 %
Nickel, Ni 35 - 40 %
35 - 40 %
Niobium, Nb (Columbium, Cb) 4.3 - 5.2 %
4.3 - 5.2 %
Silicon, Si 0.25 - 0.50 %
0.25 - 0.50 %
Titanium, Ti 1.3 - 1.8 %
1.3 - 1.8 %
Descriptive Properties Value Comments
Heat Treatment Sol. Anneal & Age