Polymer Property : Tensile Strength, Ultimate = 173300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1195 MPa

@Temperature 650 °C
173300 psi

@Temperature 1200 °F
Haynes Waspaloyâ„¢ alloy, sheet
Age-hardenable superalloy with very good strength at temperatures up 980°C (1800°F), can be cold-formed in the annealed condition, may also be hot formed at 1040°C (1900°F) and above, go..
Tensile Strength, Ultimate 1195 MPa

@Temperature 205 °C
173300 psi

@Temperature 401 °F
Haynes 242® alloy, bar and rings, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Tensile Strength, Ultimate 1195 MPa

@Temperature 95.0 °C
173300 psi

@Temperature 203 °F
Haynes 242® alloy, hot rolled plate, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good thermal..