Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1195 MPa @Temperature 650 °C |
173300 psi @Temperature 1200 °F |
|
Haynes Waspaloy™ alloy, sheet Age-hardenable superalloy with very good strength at temperatures up 980°C (1800°F), can be cold-formed in the annealed condition, may also be hot formed at 1040°C (1900°F) and above, go.. |
|||
Tensile Strength, Ultimate | 1195 MPa @Temperature 205 °C |
173300 psi @Temperature 401 °F |
|
Haynes 242® alloy, bar and rings, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Tensile Strength, Ultimate | 1195 MPa @Temperature 95.0 °C |
173300 psi @Temperature 203 °F |
|
Haynes 242® alloy, hot rolled plate, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good thermal.. |