Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1180 MPa | 171000 psi | Typical |
TIMET TIMETAL® 17 Titanium Alloy (Ti-5Al-2Sn-4Mo-2Zr-6Mo); Aged Billet/Bar Features: High strength, deep hardenable forging alloy primarily for jet engines. Allows heat treatment to a variety of strength levels in sections up to 6 inches. Offers good ductility and toughnes.. |
|||
Tensile Strength, Ultimate | 1180 MPa | 171000 psi | |
Carpenter Pyromet® CTX-3 Superalloy, Heat Treated Data provided by Carpenter Technology Corporation.Pyromet® alloy CTX-3 is a high strength, precipitation hardenable superalloy which exhibits a low CTE over a broad temperature range. This alloy a.. |
|||
Tensile Strength, Ultimate | 1179 MPa | 171000 psi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 50% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Tensile Strength, Ultimate | 1180 MPa | 171000 psi | Trans. |
ATI Wah Chang 425™ Titanium Alloy, Hot Rolled & Annealed Plate, Solution Treated Annealed ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p.. |