Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1179 MPa | 171000 psi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 50% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |