Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 164 MPa | 23800 psi | ASTM D638 |
A. Schulman ComAlloy E-16822-1B Internally Lubricated, Carbon Fiber Reinforced Nylon 6/6 Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Tensile Strength, Ultimate | 164 MPa | 23800 psi | |
AIM 70In/30Pb Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |