Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1310 - 1550 MPa | 190000 - 225000 psi | Core; Heat Treated from 1850°F |
Latrobe CBS-223â„¢ VIM-VAR Carburizing Bearing and Gear Steel CBS-223 VIM-VAR steel is a double vacuum melted carburizing steel with high hot hardness characteristics. Double vacuum melting sequentially combines vacuum induction melting with VACARCâ„¢ remel.. |
|||
Tensile Strength, Ultimate | 1350 - 1550 MPa | 196000 - 225000 psi | after modified H900 heat treatment, XY direction |
EOS PH1 Precipitation Hardening Stainless Steel for DMLS 3D Printing EOS Stainless Steel PH1 is a stainless steel powder which has been optimized especially for processing on EOSINT M 270 systems. This stainless steel prototyping material is tough and resistant to .. |
|||
Tensile Strength, Ultimate | 1350 - 1550 MPa | 196000 - 225000 psi | after modified H900 heat treatment, Z direction |
EOS PH1 Precipitation Hardening Stainless Steel for DMLS 3D Printing EOS Stainless Steel PH1 is a stainless steel powder which has been optimized especially for processing on EOSINT M 270 systems. This stainless steel prototyping material is tough and resistant to .. |