Material Notes:
CBS-223 VIM-VAR steel is a double vacuum melted carburizing steel with high hot hardness characteristics. Double vacuum melting sequentially combines vacuum induction melting with VACARCâ„¢ remelting to provide for superior cleanliness, which imparts improved fatigue strength and fracture toughness to the alloy. Its high hot hardness and the improved properties readily identify CBS-223 VIMVAR steel for use as gears, shafts and bearings in helicopter and other aerospace applications.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Density 7.75 g/cc
0.280 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 25
25
1200°F Temper
41
41
400°F Temper Temperature
46
46
950°F Temper
Tensile Strength, Ultimate 1310 - 1550 MPa
190000 - 225000 psi
Core; Heat Treated from 1850°F
Tensile Strength, Yield 1138 - 1172 MPa

@Strain 0.200 %
165100 - 170000 psi

@Strain 0.200 %
Core heat treated from 1850°F
Modulus of Elasticity 174 GPa

@Temperature 1000 °C
25300 ksi

@Temperature 1830 °F
216 GPa

@Temperature 70.0 °C
31400 ksi

@Temperature 158 °F
Thermal Properties Metric English Comments
CTE, linear 13.32 µm/m-°C

@Temperature 21.0 - 649 °C
7.400 µin/in-°F

@Temperature 69.8 - 1200 °F
14.58 µm/m-°C

@Temperature 427 - 649 °C
8.100 µin/in-°F

@Temperature 801 - 1200 °F
Component Elements Properties Metric English Comments
Carbon, C 0.14 %
0.14 %
Chromium, Cr 5.0 %
5.0 %
Iron, Fe 90.36 %
90.36 %
Manganese, Mn 0.40 %
0.40 %
Molybdenum, Mo 1.4 %
1.4 %
Silicon, Si 0.90 %
0.90 %
Tungsten, W 1.35 %
1.35 %
Vanadium, V 0.45 %
0.45 %