Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 8.80 MPa
1280 psi
ASTM D412
Multibase Multi-Flex® TPE A 7301 BLK
The data is the actual data obtained from the above sample. This material is based on Shell's Kraton G technology. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tensile Strength, Ultimate 8.83 MPa
1280 psi
no post cure, press cured for 5 minutes; ASTM D412
Multibase SILASTIC® 7-4860 Dow-Corning Biomedical Grade Liquid Silicone Rubber
Information provided by Multibase
Tensile Strength, Ultimate 8.83 MPa
1280 psi
no post cure, press cured for 5 minutes; ASTM D412
Multibase SILASTIC® 7-6830 Dow-Corning Biomedical Grade Liquid Silicone Rubber
Information provided by Multibase
Tensile Strength, Ultimate 8.83 MPa
1280 psi
no post cure; ASTM D412
Multibase C6-560 Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Ultimate 8.83 MPa
1280 psi
ASTM D412
Stellarchem SV-B75E TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..
Tensile Strength, Ultimate 8.83 MPa
1280 psi
Dow Corning C6-560 LIQUID SILICONE RUBBER KIT
Dow Corning® Class VI Elastomers are heat cured elastomer raw materials for use by customers fabricating medical devices and parts.Information provided by Dow Corning
Tensile Strength, Ultimate 8.83 MPa
1280 psi
Dow Corning SILASTIC® 7-4860 BIOMEDICAL GRADE LSR, KIT
Silastic® BioMedical Grade Liquid Silicone Rubbers are heat cured elastomer raw materials for use by customers fabricating medical devices.Information provided by Dow Corning
Tensile Strength, Ultimate 8.83 MPa
1280 psi
Dow Corning SILASTIC® 7-6830 BIOMEDICAL GRADE LSR, KIT
Silastic® BioMedical Grade Liquid Silicone Rubbers are heat cured elastomer raw materials for use by customers fabricating medical devices.Information provided by Dow Corning
Tensile Strength, Ultimate 8.80 MPa
1280 psi
ISO 527-1/-2
DSM Arnitel® XG5858 TPC-ET
Injection Molding
Tensile Strength, Ultimate 8.80 MPa
1280 psi
508 mm/min; ASTM D638
Dow Engage® 8180 Polyolefin Elastomer
Description: Engage® 8180 polyolefin elastomer is a lower density, high performance ethylene-octene copolymer that has excellent flow characteristics and provides good impact properties in blends w..
Tensile Strength, Ultimate 8.80 MPa
1280 psi
Dow LDPE 955I Low Density Polyethylene
DOW LDPE 955I resin is a medium molecular weight distribution homo polymer designed to offer excellent clarity and flexibility, and good toughness, with low warpage. Typical applications include lid..
Tensile Strength, Ultimate 8.83 MPa
1280 psi
ASTM D412; ISO 37
Advanced Polymer Alloys Alcryn® 4670 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..