Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1270 - 1560 MPa | 184000 - 226000 psi | |
Materion Beryllium Copper Alloy 25 Rod and Bar; HT (TH04) Temper; up to 9.5 mm (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Tensile Strength, Ultimate | 1270 - 1490 MPa | 184000 - 216000 psi | |
Materion Beryllium Copper Alloy 25 Strip; 1/2HT (TH02) Temper (UNS C17200) Treatment required for max strength: 2 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 73%Superficial Hardness: 30N 58-6.. |
|||
Tensile Strength, Ultimate | 1270 - 1560 MPa | 184000 - 226000 psi | |
Materion Beryllium Copper Alloy 25 Tube; HT (TH04) Temper; up to 9.5 mm o.d. (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Tensile Strength, Ultimate | 1270 - 1560 MPa | 184000 - 226000 psi | |
Materion Beryllium Copper Alloy M25 Rod and Bar; HT (TH04) Temper; up to 9.5 mm (UNS C17300) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Tensile Strength, Ultimate | 1270 - 1490 MPa | 184000 - 216000 psi | |
Materion Beryllium Copper Alloy M25 Wire; 1/2HT (TH02) Temper; 1.3-12.7 mm Diameter (UNS C17300) Treatment required for max strength: 1.5 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed.. |
|||
Tensile Strength, Ultimate | 1270 - 1560 MPa | 184000 - 226000 psi | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; up to 9.5 mm Thickness (UNS C17200) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Ultimate | 1270 - 1490 MPa | 184000 - 216000 psi | |
Materion Beryllium Copper Alloy 25 Wire; 1/2HT (TH02) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: 1.5 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed.. |
|||
Tensile Strength, Ultimate | 1270 - 1380 MPa | 184000 - 200000 psi | |
Latrobe Lescalloy® Jethete M-152 ESR 8" RCS High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â.. |
|||
Tensile Strength, Ultimate | 1270 MPa | 184000 psi | |
Haynes 242® alloy, hot rolled plate, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good thermal.. |