Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1130 - 1380 MPa | 164000 - 200000 psi | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; HT (TH04) Temper; over 25 to 51 mm Thickness (UNS C17000) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Ultimate | 1130 - 1380 MPa | 164000 - 200000 psi | |
Materion Beryllium Copper Alloy 165 Rod and Bar; HT (TH04) Temper; over 25.4 to 76 mm (UNS C17000) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Tensile Strength, Ultimate | 1130 - 1380 MPa | 164000 - 200000 psi | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; AT (TF00) Temper; All Thicknesses (UNS C17200) Treatment required for max strength: 3 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Ultimate | 1130 - 1380 MPa | 164000 - 200000 psi | |
Materion Beryllium Copper Alloy 25 Rod and Bar; AT (TF00) Temper; over 76 mm (UNS C17200) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Tensile Strength, Ultimate | 1130 - 1380 MPa | 164000 - 200000 psi | |
Materion Beryllium Copper Alloy 25 Tube; AT (TF00) Temper; over 76 mm o.d. (UNS C17200) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Tensile Strength, Ultimate | 1130 - 1380 MPa | 164000 - 200000 psi | |
Materion Beryllium Copper Alloy M25 Rod and Bar; AT (TF00) Temper; up to 76 mm (UNS C17300) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Tensile Strength, Ultimate | 1130 - 1380 MPa | 164000 - 200000 psi | |
Materion Beryllium Copper Alloy 25 Rod and Bar; AT (TF00) Temper; up to 76 mm (UNS C17200) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Tensile Strength, Ultimate | 1130 - 1380 MPa | 164000 - 200000 psi | |
Materion Beryllium Copper Alloy 25 Tube; AT (TF00) Temper; up to 76 mm o.d. (UNS C17200) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Tensile Strength, Ultimate | 1130 - 1380 MPa | 164000 - 200000 psi | |
Materion Beryllium Copper Alloy M25 Rod and Bar; AT (TF00) Temper; over 76 mm (UNS C17300) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Tensile Strength, Ultimate | 1270 - 1380 MPa | 184000 - 200000 psi | |
Latrobe Lescalloy® Jethete M-152 ESR 8" RCS High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â.. |
|||
Tensile Strength, Ultimate | 1100 - 1380 MPa | 160000 - 200000 psi | |
Special Metals DURANICKEL® 301 (UNS N03301) Hot-Finished and Aged Rod and Bar Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Hot-Finished and Aged Rod and Bar specifically. Other property values are typical of aged DURANIC.. |
|||
Tensile Strength, Ultimate | 1100 - 1380 MPa | 160000 - 200000 psi | |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Wire Tensile strength (ultimate) and elongation values reported here are typical for Spring Wire specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the alloy in gener.. |