Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1245 MPa @Temperature 95.0 °C |
180600 psi @Temperature 203 °F |
|
Haynes 242® alloy, bar and rings, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Tensile Strength, Ultimate | 1245 MPa | 180500 psi | |
Special Metals INCONEL® 706 Precipitation Hardening Alloy, Forged Disc, 3 Part Heat Treatment Tensile strength (ultimate and yield), reduction of area, and elongation values reported here are typical for Forged Disc, 3 Part Heat Treatment samples. Density and magnetic permeability are typica.. |