Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 8.14 MPa | 1180 psi | |
Dow Corning SILASTIC® Q7-4535 BIOMEDICAL GRADE ETR ELASTOMER One-part, enhanced tear-resistant silicone elastomers; uncatalyzed (customer selects peroxide catalyst) elastomer materials designed for compounding into elastomer for part fabrication and medical d.. |