Tensile Strength, Ultimate 698 MPa

@Diameter 12.7 mm
101000 psi

@Diameter 0.500 in
Kaiser 7068 T6, T651 Rod & Bar
Alloy 7068 offers some of the highest strength mechanical properties available in an extruded product. Intended for aerospace, ordnance and light weight recreational applications where extremely hig..
Tensile Strength, Ultimate 696 MPa

@Temperature 23.0 °C
101000 psi

@Temperature 73.4 °F
Lucas-Milhaupt EASY FLO Silver Based Cadmium-Bearing Filler Metal
Applications: Easy-Flo is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wettin..
Tensile Strength, Ultimate 696 MPa
101000 psi
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GMAW spray weld 1.1 mm diameter filler wire
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Tensile Strength, Ultimate 696 MPa
101000 psi
Universal Wire Works No. 21 Cobalt Alloy Welding Wire
Universal No. 21 is a cobalt-chromium-molybdenum alloy designed for covered electrode, TIG, MIG, hard surfacing applications. The work-hardening characteristics, high ductility properties, excellent..
Tensile Strength, Ultimate 696 - 779 MPa
101000 - 113000 psi
Eagle Brass 64725 MAX251C, Spring
Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In..
Tensile Strength, Ultimate 696 - 786 MPa
101000 - 114000 psi
Eagle Brass 762 Nickel Silver 12%, Extra Hard
762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s..
Tensile Strength, Ultimate 696 MPa
101000 psi
Ametek High Purity Nickel Strip 899D 50% Cold-Rolled
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Tensile Strength, Ultimate 696 MPa
101000 psi
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GTAW short arc weld 1.1 mm diameter filler wire
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin..