Universal Wire Works No. 21 Cobalt Alloy Welding Wire

Category Metal , Nonferrous Metal , Cobalt Alloy , Superalloy
Manufacturer Universal Wire Works
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works No. 21 Cobalt Alloy Welding Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Universal No. 21 is a cobalt-chromium-molybdenum alloy designed for covered electrode, TIG, MIG, hard surfacing applications. The work-hardening characteristics, high ductility properties, excellent resistance to impact and metal to metal wear suit Universal 21 to severe applications where a work-hardening material is desired (as welded Rc 20; work hardened Rc 40 - 43).Universal 21 applications include: high temperature valves, high pressure valves, hot punches crushing knives, drop forging dies, tap hole augers, pump shafts and sleeves, press dies, vapor tight valve seats.Alloy 21 work hardens in service, has excellent erosion, corrosion and metal to metal wear resistance. Deposits exhibit effective hardness and a good cutting edge at high temperatures. On thick overlays Alloy 21 can be used as a buildup prior to depositing a higher hardness alloy.Machinability: Use carbide tools.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Hardness, Rockwell C 20
20
As Welded
40 - 43
40 - 43
Work Hardened
Tensile Strength, Ultimate 696 MPa
101000 psi
Thermal Properties Metric English Comments
Melting Point 1352 °C
2465 °F
Component Elements Properties Metric English Comments
Carbon, C 0.65 %
0.65 %
Chromium, Cr 28.5 %
28.5 %
Cobalt, Co 59.9 %
59.9 %
As remainder
Iron, Fe 2.0 %
2.0 %
Molybdenum, Mo 5.5 %
5.5 %
Nickel, Ni 2.0 %
2.0 %
Silicon, Si 1.0 %
1.0 %
Tungsten, W 0.50 %
0.50 %