Mechanical Properties Metric English Comments
Falling Dart Impact 12.4 J
9.15 ft-lb
ASTM D3763
LNP Thermocomp® EF-1006 BK8-114 Polyetherimide, Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..