Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 12.4 J | 9.15 ft-lb | ASTM D3763 |
LNP Thermocomp® EF-1006 BK8-114 Polyetherimide, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |